Stress corrosion of the Mg-Zn-Zr alloy system using C-ring tests

Publikation: Beiträge in SammelwerkenAufsätze in KonferenzbändenForschungbegutachtet

Standard

Stress corrosion of the Mg-Zn-Zr alloy system using C-ring tests. / Maier, Petra; Ostermeier, Nico; Wicke, Jens et al.
MS and T 2019 - Materials Science and Technology 2019. Materials Science and Technology (MS&T), 2019. S. 1142-1149.

Publikation: Beiträge in SammelwerkenAufsätze in KonferenzbändenForschungbegutachtet

Harvard

Maier, P, Ostermeier, N, Wicke, J, You, S & Hort, N 2019, Stress corrosion of the Mg-Zn-Zr alloy system using C-ring tests. in MS and T 2019 - Materials Science and Technology 2019. Materials Science and Technology (MS&T), S. 1142-1149, Technical Meeting and Exhibition on Materials Science and Technology - MS & T 2019, Portland, USA / Vereinigte Staaten, 29.09.19. https://doi.org/10.7449/2019/MST_2019_1142_1149

APA

Maier, P., Ostermeier, N., Wicke, J., You, S., & Hort, N. (2019). Stress corrosion of the Mg-Zn-Zr alloy system using C-ring tests. In MS and T 2019 - Materials Science and Technology 2019 (S. 1142-1149). Materials Science and Technology (MS&T). https://doi.org/10.7449/2019/MST_2019_1142_1149

Vancouver

Maier P, Ostermeier N, Wicke J, You S, Hort N. Stress corrosion of the Mg-Zn-Zr alloy system using C-ring tests. in MS and T 2019 - Materials Science and Technology 2019. Materials Science and Technology (MS&T). 2019. S. 1142-1149 doi: 10.7449/2019/MST_2019_1142_1149

Bibtex

@inbook{594064971c9a4e8c91a6b2556fb0d717,
title = "Stress corrosion of the Mg-Zn-Zr alloy system using C-ring tests",
abstract = "This study focuses on the stress corrosion behavior of the Mg-Zn-Zr alloy system in extruded condition (tubes). The binary alloys Mg-Zn and Mg-Zr are compared to the ternary alloy system regarding microstructure, hardness, bending strength and corrosion behavior. C-ring tests in Ringer solution are used to evaluate the stress corrosion properties. POM polymer, being corrosion resistant and neutral to the Mg-corrosion, was chosen to build up the test set-up for the C-ring tests. Bending tests have been done to determine the elastic-plastic region of the samples - before starting the C-ring experiments. Twinning as a result of deformation increases the corrosion rate and is most prominent at the Mg-Zr alloy. Signs of pitting corrosion to different extents have been found in all alloys investigated. The Mg-Zn alloy corrodes the most within this alloy group. Plastic deformation is increasing the corrosion, however, signs of stress corrosion cracking could not be found.",
keywords = "C-ring test, Corrosion morphology, Magnesium, Mg-Zn-Zr, Stress corrosion, Engineering",
author = "Petra Maier and Nico Ostermeier and Jens Wicke and Sihang You and Norbert Hort",
year = "2019",
doi = "10.7449/2019/MST_2019_1142_1149",
language = "English",
isbn = "9780873397704",
pages = "1142--1149",
booktitle = "MS and T 2019 - Materials Science and Technology 2019",
publisher = "Materials Science and Technology (MS&T)",
address = "United States",
note = "Technical Meeting and Exhibition on Materials Science and Technology - MS & T 2019, MS & T 2019 ; Conference date: 29-09-2019 Through 03-10-2019",
url = "https://www.matscitech.org/MST19/",

}

RIS

TY - CHAP

T1 - Stress corrosion of the Mg-Zn-Zr alloy system using C-ring tests

AU - Maier, Petra

AU - Ostermeier, Nico

AU - Wicke, Jens

AU - You, Sihang

AU - Hort, Norbert

PY - 2019

Y1 - 2019

N2 - This study focuses on the stress corrosion behavior of the Mg-Zn-Zr alloy system in extruded condition (tubes). The binary alloys Mg-Zn and Mg-Zr are compared to the ternary alloy system regarding microstructure, hardness, bending strength and corrosion behavior. C-ring tests in Ringer solution are used to evaluate the stress corrosion properties. POM polymer, being corrosion resistant and neutral to the Mg-corrosion, was chosen to build up the test set-up for the C-ring tests. Bending tests have been done to determine the elastic-plastic region of the samples - before starting the C-ring experiments. Twinning as a result of deformation increases the corrosion rate and is most prominent at the Mg-Zr alloy. Signs of pitting corrosion to different extents have been found in all alloys investigated. The Mg-Zn alloy corrodes the most within this alloy group. Plastic deformation is increasing the corrosion, however, signs of stress corrosion cracking could not be found.

AB - This study focuses on the stress corrosion behavior of the Mg-Zn-Zr alloy system in extruded condition (tubes). The binary alloys Mg-Zn and Mg-Zr are compared to the ternary alloy system regarding microstructure, hardness, bending strength and corrosion behavior. C-ring tests in Ringer solution are used to evaluate the stress corrosion properties. POM polymer, being corrosion resistant and neutral to the Mg-corrosion, was chosen to build up the test set-up for the C-ring tests. Bending tests have been done to determine the elastic-plastic region of the samples - before starting the C-ring experiments. Twinning as a result of deformation increases the corrosion rate and is most prominent at the Mg-Zr alloy. Signs of pitting corrosion to different extents have been found in all alloys investigated. The Mg-Zn alloy corrodes the most within this alloy group. Plastic deformation is increasing the corrosion, however, signs of stress corrosion cracking could not be found.

KW - C-ring test

KW - Corrosion morphology

KW - Magnesium

KW - Mg-Zn-Zr

KW - Stress corrosion

KW - Engineering

UR - http://www.scopus.com/inward/record.url?scp=85075403862&partnerID=8YFLogxK

U2 - 10.7449/2019/MST_2019_1142_1149

DO - 10.7449/2019/MST_2019_1142_1149

M3 - Article in conference proceedings

AN - SCOPUS:85075403862

SN - 9780873397704

SN - 0873397703

SP - 1142

EP - 1149

BT - MS and T 2019 - Materials Science and Technology 2019

PB - Materials Science and Technology (MS&T)

T2 - Technical Meeting and Exhibition on Materials Science and Technology - MS & T 2019

Y2 - 29 September 2019 through 3 October 2019

ER -

DOI

Zuletzt angesehen

Publikationen

  1. Positional income concerns and personality
  2. Algae Cultivation as Measure for the Sanitation of Organic Waste—A Case Study Based on the Alga Galdieria sulphuraria Grown on Food Waste Hydrolysate in a Continuous Flow Culture
  3. WIATEC - a world integrated assessment model of global trade environment and climate change
  4. Internetbasierte Selbsthilfeprogramme unterstützen die Behandlung: depressive Störungen
  5. Saproxylic beetles in the Gartow region of Lower Saxony, a hotspot of invertebrate diversity in north-western Germany
  6. Der Ozean im Glas
  7. Biodiversity assessments
  8. Seth Price. Decimating Digital Data
  9. Trouble on my mind
  10. Too Scared to Fight Back? Affective Job Insecurity as a Boundary Condition Between Workplace Incivility and Negative Mood States in Temporary Agency Workers
  11. Length measurement and estimation in primary school
  12. Paul Bourget
  13. Einleitung
  14. Markteintritte, Marktaustritte und Produktivität
  15. Shedding Some Light on Economics in Philippians
  16. Cognition, consciousness and business ethics - the role of implicit social cognition in moral management behaviour
  17. Alltägliche Unterrichtsplanung und -analyse in konstruktivistischer Perspektive
  18. Psychometric Properties of the Online Arabic Versions of BDI-II, HSCL-25, and PDS
  19. Öffentlicher Raum
  20. Biogeographical patterns in the diet of the wildcat, Felis silvestris Schreber, in Eurasia: Factors affecting the trophic diversity
  21. Preferences for health insurance and health status
  22. Eco-Control para la Gestión Ambiental
  23. Species-specific responses of wood growth to flooding and climate in floodplain forests in central Germany
  24. Fragenbox Mathematik
  25. Which is the ‘right’ choice of the market portfolio of the CAPM?
  26. Kontextualisierung im nicht-präferierten Format
  27. Crises and Entrepreneurial Opportunities
  28. Repatriate knowledge transfer