A critical review of the Stress Corrosion Cracking (SCC) of magnesium alloys
Publikation: Beiträge in Zeitschriften › Übersichtsarbeiten › Forschung
Standard
in: Advanced Engineering Materials, Jahrgang 7, Nr. 8, 01.08.2005, S. 659-693.
Publikation: Beiträge in Zeitschriften › Übersichtsarbeiten › Forschung
Harvard
APA
Vancouver
Bibtex
}
RIS
TY - JOUR
T1 - A critical review of the Stress Corrosion Cracking (SCC) of magnesium alloys
AU - Winzer, Nicholas
AU - Atrens, Andrej
AU - Song, Guangling
AU - Ghali, Edward
AU - Dietzel, Wolfgang
AU - Kainer, Karl Ulrich
AU - Hort, Norbert
AU - Blawert, Carsten
PY - 2005/8/1
Y1 - 2005/8/1
N2 - This review aims to provide a foundation for the safe and effective use of magnesium (Mg) alloys, including practical guidelines for the service use of Mg alloys in the atmosphere and/or in contact with aqueous solutions. This is to provide support for the rapidly increasing use of Mg in industrial applications, particularly in the automobile industry. These guidelines should be firmly based on a critical analysis of our knowledge of SCC based on (1) service experience, (2) laboratory testing and (3) understanding of the mechanism of SCC, as well as based on an understanding of the Mg corrosion mechanism.
AB - This review aims to provide a foundation for the safe and effective use of magnesium (Mg) alloys, including practical guidelines for the service use of Mg alloys in the atmosphere and/or in contact with aqueous solutions. This is to provide support for the rapidly increasing use of Mg in industrial applications, particularly in the automobile industry. These guidelines should be firmly based on a critical analysis of our knowledge of SCC based on (1) service experience, (2) laboratory testing and (3) understanding of the mechanism of SCC, as well as based on an understanding of the Mg corrosion mechanism.
KW - Engineering
UR - http://www.scopus.com/inward/record.url?scp=25444458037&partnerID=8YFLogxK
UR - https://www.mendeley.com/catalogue/b985e624-556d-3e2b-9326-1aeac808b988/
U2 - 10.1002/adem.200500071
DO - 10.1002/adem.200500071
M3 - Scientific review articles
AN - SCOPUS:25444458037
VL - 7
SP - 659
EP - 693
JO - Advanced Engineering Materials
JF - Advanced Engineering Materials
SN - 1438-1656
IS - 8
ER -