Anisotropy and size effect in tensile mechanical properties of Al-Cu-Li 2198 alloy
Research output: Journal contributions › Journal articles › Research › peer-review
Standard
In: Procedia Structural Integrity, Vol. 5, 01.01.2017, p. 13-18.
Research output: Journal contributions › Journal articles › Research › peer-review
Harvard
APA
Vancouver
Bibtex
}
RIS
TY - JOUR
T1 - Anisotropy and size effect in tensile mechanical properties of Al-Cu-Li 2198 alloy
AU - Examilioto, Theano
AU - Klusemann, Benjamin
AU - Kashaev, Nikolai
AU - Riekehr, Stefan
AU - Enz, Josephin
AU - Alexopoulos, Nikolaos
N1 - Part of special issue: 2nd International Conference on Structural Integrity, ICSI 2017, 4-7 September 2017, Funchal, Madeira, Portugal Publisher Copyright: © 2017 EW MATERIALS. All rights reserved.
PY - 2017/1/1
Y1 - 2017/1/1
N2 - The anisotropy effect on tensile mechanical properties of an Al-Cu-Li (2198) alloy with regard to thickness of the specimens under different ageing conditions was investigated. Occurring size effects between macro and micro (0.5, 3.2 and 5.0 mm thickness and 10 and 50 mm gauge length) tensile specimens was discussed. The mechanical behavior of AA2198 was examined by taking into account the experimental results from micro-flat and standard tensile specimens. Higher thickness specimens showed higher elongation at fracture values and slightly lower yield stress properties. Anisotropy seems to be higher at T3 condition, while the lowest was noticed at the peak-ageing condition. The results showed that the micro-flat tensile specimens in T3 condition presented slightly lower yield stress (10 MPa difference) and essentially lower elongation at fracture values (more than 40 % decrease), when compared with the respective of higher thickness specimens. It was also shown that thicker (5.0 mm) specimens exhibit slightly higher tensile ductility properties (almost 17 %) and slightly lower tensile strength properties than the respective 3.2 mm thickness specimens. There is evidence of relative difference in mechanical properties due to the rolling process in the two sheet directions (L and T directions); such anisotropy difference seems to be marginal at the peak-ageing condition.
AB - The anisotropy effect on tensile mechanical properties of an Al-Cu-Li (2198) alloy with regard to thickness of the specimens under different ageing conditions was investigated. Occurring size effects between macro and micro (0.5, 3.2 and 5.0 mm thickness and 10 and 50 mm gauge length) tensile specimens was discussed. The mechanical behavior of AA2198 was examined by taking into account the experimental results from micro-flat and standard tensile specimens. Higher thickness specimens showed higher elongation at fracture values and slightly lower yield stress properties. Anisotropy seems to be higher at T3 condition, while the lowest was noticed at the peak-ageing condition. The results showed that the micro-flat tensile specimens in T3 condition presented slightly lower yield stress (10 MPa difference) and essentially lower elongation at fracture values (more than 40 % decrease), when compared with the respective of higher thickness specimens. It was also shown that thicker (5.0 mm) specimens exhibit slightly higher tensile ductility properties (almost 17 %) and slightly lower tensile strength properties than the respective 3.2 mm thickness specimens. There is evidence of relative difference in mechanical properties due to the rolling process in the two sheet directions (L and T directions); such anisotropy difference seems to be marginal at the peak-ageing condition.
KW - Engineering
KW - alluminion alloy
KW - anisotropy effect
KW - tensible mechanical properties
KW - size effect
UR - http://www.scopus.com/inward/record.url?scp=85063132652&partnerID=8YFLogxK
U2 - 10.1016/j.prostr.2017.07.052
DO - 10.1016/j.prostr.2017.07.052
M3 - Journal articles
VL - 5
SP - 13
EP - 18
JO - Procedia Structural Integrity
JF - Procedia Structural Integrity
SN - 2452-3216
ER -