Influence of zinc and silver additions on hot tearing susceptibility of Mg-14Gd-0.4Zr alloy

Publikation: Beiträge in ZeitschriftenZeitschriftenaufsätzeForschungbegutachtet

Standard

Influence of zinc and silver additions on hot tearing susceptibility of Mg-14Gd-0.4Zr alloy. / Yang, Lixiang; Wang, Shaozhu; Huang, Yuanding et al.
in: Journal of Rare Earths, 24.04.2024.

Publikation: Beiträge in ZeitschriftenZeitschriftenaufsätzeForschungbegutachtet

Harvard

Yang, L, Wang, S, Huang, Y, Hou, Z, Wu, H, Dong, X, Shi, H, Zou, W, Li, D, Li, F, Sun, B, Li, Z, Hort, N & Xiao, L 2024, 'Influence of zinc and silver additions on hot tearing susceptibility of Mg-14Gd-0.4Zr alloy', Journal of Rare Earths. https://doi.org/10.1016/j.jre.2024.04.017

APA

Yang, L., Wang, S., Huang, Y., Hou, Z., Wu, H., Dong, X., Shi, H., Zou, W., Li, D., Li, F., Sun, B., Li, Z., Hort, N., & Xiao, L. (2024). Influence of zinc and silver additions on hot tearing susceptibility of Mg-14Gd-0.4Zr alloy. Journal of Rare Earths. Vorzeitige Online-Publikation. https://doi.org/10.1016/j.jre.2024.04.017

Vancouver

Yang L, Wang S, Huang Y, Hou Z, Wu H, Dong X et al. Influence of zinc and silver additions on hot tearing susceptibility of Mg-14Gd-0.4Zr alloy. Journal of Rare Earths. 2024 Apr 24. Epub 2024 Apr 24. doi: 10.1016/j.jre.2024.04.017

Bibtex

@article{485ab748b612412eaa03f1b229f7c5fd,
title = "Influence of zinc and silver additions on hot tearing susceptibility of Mg-14Gd-0.4Zr alloy",
abstract = "The effects of 1Zn and/or 2Ag additions on the hot tearing susceptibility (HTS) of Mg-14Gd-0.4Zr (wt%) alloy were studied. The HTS was evaluated by both theoretical predictions using Kou's criterion and experimental observations based on the in situ force-temperature recorded constrained rod casting (ISFTCRC) method. The results show that the order of HTS from high to low is Mg-14Gd-2Ag–1Zn-0.4Zr, Mg-14Gd-2Ag-0.4Zr, Mg-14Gd-1Zn-0.4Zr and Mg-14Gd-0.4Zr. Adding 1Zn and/or 2Ag changes the solidification path and the solidification interval, which affects the hot tearing susceptibility. Alloying elemental 1Zn slightly increases the solidification interval and the temperature range in the square root of the solid phase fraction (ƒs1/2) range of 0.949–0.995, resulting in a slight increase in the hot tearing susceptibility. The addition of 2Ag drastically widens both the solidification interval and the temperature range in the ƒs1/2 range of 0.949–0.995, thus significantly increasing the hot tearing susceptibility. Compared to the addition of 2Ag alone, the broadening degree of both the solidification interval and the temperature range in the ƒs1/2 range of 0.949–0.995 is greater by adding the composite 2Ag/1Zn, which further promotes the occurrence of hot tearing. A narrower solidification interval and a temperature range in the ƒs1/2 range of 0.949–0.995 result in a lower hot tearing susceptibility.",
keywords = "Differential scanning calorimetry/thermal gravimetric (DSC/TG), Hot tearing, Mg-Gd-Ag/Zn, Rare earths, Solidification interval, Solidification path, Engineering",
author = "Lixiang Yang and Shaozhu Wang and Yuanding Huang and Zhengquan Hou and Hai Wu and Xiwang Dong and Hui Shi and Wenbing Zou and Dejiang Li and Fei Li and Baode Sun and Zhongquan Li and Norbert Hort and Lv Xiao",
note = "Publisher Copyright: {\textcopyright} 2024 Chinese Society of Rare Earths",
year = "2024",
month = apr,
day = "24",
doi = "10.1016/j.jre.2024.04.017",
language = "English",
journal = "Journal of Rare Earths",
issn = "1002-0721",
publisher = "Chinese Rare Earth Society",

}

RIS

TY - JOUR

T1 - Influence of zinc and silver additions on hot tearing susceptibility of Mg-14Gd-0.4Zr alloy

AU - Yang, Lixiang

AU - Wang, Shaozhu

AU - Huang, Yuanding

AU - Hou, Zhengquan

AU - Wu, Hai

AU - Dong, Xiwang

AU - Shi, Hui

AU - Zou, Wenbing

AU - Li, Dejiang

AU - Li, Fei

AU - Sun, Baode

AU - Li, Zhongquan

AU - Hort, Norbert

AU - Xiao, Lv

N1 - Publisher Copyright: © 2024 Chinese Society of Rare Earths

PY - 2024/4/24

Y1 - 2024/4/24

N2 - The effects of 1Zn and/or 2Ag additions on the hot tearing susceptibility (HTS) of Mg-14Gd-0.4Zr (wt%) alloy were studied. The HTS was evaluated by both theoretical predictions using Kou's criterion and experimental observations based on the in situ force-temperature recorded constrained rod casting (ISFTCRC) method. The results show that the order of HTS from high to low is Mg-14Gd-2Ag–1Zn-0.4Zr, Mg-14Gd-2Ag-0.4Zr, Mg-14Gd-1Zn-0.4Zr and Mg-14Gd-0.4Zr. Adding 1Zn and/or 2Ag changes the solidification path and the solidification interval, which affects the hot tearing susceptibility. Alloying elemental 1Zn slightly increases the solidification interval and the temperature range in the square root of the solid phase fraction (ƒs1/2) range of 0.949–0.995, resulting in a slight increase in the hot tearing susceptibility. The addition of 2Ag drastically widens both the solidification interval and the temperature range in the ƒs1/2 range of 0.949–0.995, thus significantly increasing the hot tearing susceptibility. Compared to the addition of 2Ag alone, the broadening degree of both the solidification interval and the temperature range in the ƒs1/2 range of 0.949–0.995 is greater by adding the composite 2Ag/1Zn, which further promotes the occurrence of hot tearing. A narrower solidification interval and a temperature range in the ƒs1/2 range of 0.949–0.995 result in a lower hot tearing susceptibility.

AB - The effects of 1Zn and/or 2Ag additions on the hot tearing susceptibility (HTS) of Mg-14Gd-0.4Zr (wt%) alloy were studied. The HTS was evaluated by both theoretical predictions using Kou's criterion and experimental observations based on the in situ force-temperature recorded constrained rod casting (ISFTCRC) method. The results show that the order of HTS from high to low is Mg-14Gd-2Ag–1Zn-0.4Zr, Mg-14Gd-2Ag-0.4Zr, Mg-14Gd-1Zn-0.4Zr and Mg-14Gd-0.4Zr. Adding 1Zn and/or 2Ag changes the solidification path and the solidification interval, which affects the hot tearing susceptibility. Alloying elemental 1Zn slightly increases the solidification interval and the temperature range in the square root of the solid phase fraction (ƒs1/2) range of 0.949–0.995, resulting in a slight increase in the hot tearing susceptibility. The addition of 2Ag drastically widens both the solidification interval and the temperature range in the ƒs1/2 range of 0.949–0.995, thus significantly increasing the hot tearing susceptibility. Compared to the addition of 2Ag alone, the broadening degree of both the solidification interval and the temperature range in the ƒs1/2 range of 0.949–0.995 is greater by adding the composite 2Ag/1Zn, which further promotes the occurrence of hot tearing. A narrower solidification interval and a temperature range in the ƒs1/2 range of 0.949–0.995 result in a lower hot tearing susceptibility.

KW - Differential scanning calorimetry/thermal gravimetric (DSC/TG)

KW - Hot tearing

KW - Mg-Gd-Ag/Zn

KW - Rare earths

KW - Solidification interval

KW - Solidification path

KW - Engineering

UR - http://www.scopus.com/inward/record.url?scp=85200113618&partnerID=8YFLogxK

UR - https://www.mendeley.com/catalogue/5dbdc232-702d-39fe-a165-480b297ca602/

U2 - 10.1016/j.jre.2024.04.017

DO - 10.1016/j.jre.2024.04.017

M3 - Journal articles

AN - SCOPUS:85200113618

JO - Journal of Rare Earths

JF - Journal of Rare Earths

SN - 1002-0721

ER -

DOI